Erbium fiber gain from the Giles parameters shipped with OptiCommPy (GPL-3.0), https://github.com/edsonportosilva/OptiCommPy, average inversion 0.70 Wavelength (nm) Gain (dB) 1528.0 23.701 1528.2 23.901 1528.4 24.091 1528.6 24.270 1528.8 24.439 1529.0 24.596 1529.2 24.742 1529.4 24.877 1529.6 25.000 1529.8 25.111 1530.0 25.210 1530.2 25.296 1530.4 25.370 1530.6 25.430 1530.8 25.476 1531.0 25.508 1531.2 25.527 1531.4 25.531 1531.6 25.520 1531.8 25.494 1532.0 25.454 1532.2 25.399 1532.4 25.329 1532.6 25.245 1532.8 25.146 1533.0 25.034 1533.2 24.909 1533.4 24.771 1533.6 24.622 1533.8 24.462 1534.0 24.294 1534.2 24.117 1534.4 23.935 1534.6 23.748 1534.8 23.558 1535.0 23.368 1535.2 23.178 1535.4 22.991 1535.6 22.809 1535.8 22.632 1536.0 22.462 1536.2 22.301 1536.4 22.149 1536.6 22.008 1536.8 21.878 1537.0 21.760 1537.2 21.655 1537.4 21.562 1537.6 21.482 1537.8 21.415 1538.0 21.360 1538.2 21.316 1538.4 21.283 1538.6 21.261 1538.8 21.248 1539.0 21.244 1539.2 21.248 1539.4 21.259 1539.6 21.277 1539.8 21.301 1540.0 21.329 1540.2 21.362 1540.4 21.399 1540.6 21.438 1540.8 21.479 1541.0 21.522 1541.2 21.566 1541.4 21.610 1541.6 21.654 1541.8 21.697 1542.0 21.739 1542.2 21.779 1542.4 21.817 1542.6 21.854 1542.8 21.889 1543.0 21.921 1543.2 21.950 1543.4 21.978 1543.6 22.002 1543.8 22.024 1544.0 22.044 1544.2 22.060 1544.4 22.074 1544.6 22.086 1544.8 22.095 1545.0 22.102 1545.2 22.107 1545.4 22.110 1545.6 22.112 1545.8 22.112 1546.0 22.110 1546.2 22.108 1546.4 22.105 1546.6 22.101 1546.8 22.096 1547.0 22.090 1547.2 22.084 1547.4 22.077 1547.6 22.070 1547.8 22.063 1548.0 22.055 1548.2 22.048 1548.4 22.040 1548.6 22.033 1548.8 22.027 1549.0 22.021 1549.2 22.016 1549.4 22.011 1549.6 22.007 1549.8 22.003 1550.0 22.000 1550.2 21.997 1550.4 21.994 1550.6 21.992 1550.8 21.991 1551.0 21.990 1551.2 21.990 1551.4 21.991 1551.6 21.993 1551.8 21.996 1552.0 22.000 1552.2 22.005 1552.4 22.011 1552.6 22.016 1552.8 22.023 1553.0 22.029 1553.2 22.035 1553.4 22.042 1553.6 22.048 1553.8 22.054 1554.0 22.060 1554.2 22.066 1554.4 22.071 1554.6 22.076 1554.8 22.081 1555.0 22.085 1555.2 22.088 1555.4 22.090 1555.6 22.091 1555.8 22.089 1556.0 22.086 1556.2 22.081 1556.4 22.074 1556.6 22.065 1556.8 22.053 1557.0 22.039 1557.2 22.022 1557.4 22.004 1557.6 21.982 1557.8 21.958 1558.0 21.931 1558.2 21.901 1558.4 21.868 1558.6 21.832 1558.8 21.793 1559.0 21.751 1559.2 21.707 1559.4 21.659 1559.6 21.609 1559.8 21.555 1560.0 21.499 1560.2 21.439 1560.4 21.376 1560.6 21.309 1560.8 21.238 1561.0 21.163 1561.2 21.083 1561.4 21.000 1561.6 20.913 1561.8 20.823 1562.0 20.729 1562.2 20.633 1562.4 20.535 1562.6 20.433 1562.8 20.329 1563.0 20.223