Erbium fiber gain from the Giles parameters shipped with OptiCommPy (GPL-3.0), https://github.com/edsonportosilva/OptiCommPy, average inversion 0.75 Wavelength (nm) Gain (dB) 1528.0 25.881 1528.2 26.070 1528.4 26.247 1528.6 26.413 1528.8 26.567 1529.0 26.709 1529.2 26.839 1529.4 26.956 1529.6 27.060 1529.8 27.152 1530.0 27.229 1530.2 27.294 1530.4 27.344 1530.6 27.380 1530.8 27.402 1531.0 27.408 1531.2 27.400 1531.4 27.376 1531.6 27.337 1531.8 27.282 1532.0 27.211 1532.2 27.125 1532.4 27.023 1532.6 26.906 1532.8 26.775 1533.0 26.629 1533.2 26.469 1533.4 26.297 1533.6 26.113 1533.8 25.918 1534.0 25.714 1534.2 25.503 1534.4 25.285 1534.6 25.063 1534.8 24.839 1535.0 24.615 1535.2 24.392 1535.4 24.172 1535.6 23.957 1535.8 23.749 1536.0 23.549 1536.2 23.358 1536.4 23.178 1536.6 23.009 1536.8 22.853 1537.0 22.710 1537.2 22.580 1537.4 22.464 1537.6 22.362 1537.8 22.272 1538.0 22.196 1538.2 22.132 1538.4 22.080 1538.6 22.039 1538.8 22.008 1539.0 21.986 1539.2 21.973 1539.4 21.967 1539.6 21.969 1539.8 21.976 1540.0 21.989 1540.2 22.007 1540.4 22.028 1540.6 22.053 1540.8 22.080 1541.0 22.108 1541.2 22.138 1541.4 22.167 1541.6 22.197 1541.8 22.226 1542.0 22.254 1542.2 22.280 1542.4 22.305 1542.6 22.328 1542.8 22.348 1543.0 22.367 1543.2 22.383 1543.4 22.396 1543.6 22.407 1543.8 22.415 1544.0 22.421 1544.2 22.424 1544.4 22.424 1544.6 22.422 1544.8 22.418 1545.0 22.412 1545.2 22.403 1545.4 22.393 1545.6 22.381 1545.8 22.368 1546.0 22.354 1546.2 22.338 1546.4 22.322 1546.6 22.305 1546.8 22.287 1547.0 22.269 1547.2 22.250 1547.4 22.231 1547.6 22.212 1547.8 22.192 1548.0 22.172 1548.2 22.153 1548.4 22.133 1548.6 22.115 1548.8 22.096 1549.0 22.079 1549.2 22.062 1549.4 22.045 1549.6 22.030 1549.8 22.015 1550.0 22.000 1550.2 21.986 1550.4 21.972 1550.6 21.959 1550.8 21.947 1551.0 21.935 1551.2 21.925 1551.4 21.915 1551.6 21.907 1551.8 21.899 1552.0 21.893 1552.2 21.887 1552.4 21.882 1552.6 21.877 1552.8 21.873 1553.0 21.870 1553.2 21.866 1553.4 21.863 1553.6 21.859 1553.8 21.856 1554.0 21.852 1554.2 21.848 1554.4 21.844 1554.6 21.839 1554.8 21.834 1555.0 21.829 1555.2 21.823 1555.4 21.816 1555.6 21.807 1555.8 21.797 1556.0 21.785 1556.2 21.771 1556.4 21.755 1556.6 21.737 1556.8 21.717 1557.0 21.694 1557.2 21.670 1557.4 21.643 1557.6 21.613 1557.8 21.581 1558.0 21.546 1558.2 21.508 1558.4 21.468 1558.6 21.425 1558.8 21.378 1559.0 21.329 1559.2 21.277 1559.4 21.223 1559.6 21.166 1559.8 21.105 1560.0 21.042 1560.2 20.976 1560.4 20.907 1560.6 20.833 1560.8 20.756 1561.0 20.675 1561.2 20.591 1561.4 20.503 1561.6 20.411 1561.8 20.316 1562.0 20.218 1562.2 20.117 1562.4 20.014 1562.6 19.909 1562.8 19.801 1563.0 19.691