Target attenuation for the first erbium fiber gain curve (n2 0.70), positive dB = loss Wavelength (nm) Attenuation (dB) 1528.0 3.478 1528.2 3.678 1528.4 3.868 1528.6 4.047 1528.8 4.216 1529.0 4.373 1529.2 4.519 1529.4 4.654 1529.6 4.777 1529.8 4.888 1530.0 4.987 1530.2 5.073 1530.4 5.147 1530.6 5.207 1530.8 5.253 1531.0 5.285 1531.2 5.304 1531.4 5.308 1531.6 5.297 1531.8 5.271 1532.0 5.231 1532.2 5.176 1532.4 5.106 1532.6 5.022 1532.8 4.923 1533.0 4.811 1533.2 4.686 1533.4 4.548 1533.6 4.399 1533.8 4.239 1534.0 4.071 1534.2 3.894 1534.4 3.712 1534.6 3.525 1534.8 3.335 1535.0 3.145 1535.2 2.955 1535.4 2.768 1535.6 2.586 1535.8 2.409 1536.0 2.239 1536.2 2.078 1536.4 1.926 1536.6 1.785 1536.8 1.655 1537.0 1.537 1537.2 1.432 1537.4 1.339 1537.6 1.259 1537.8 1.192 1538.0 1.137 1538.2 1.093 1538.4 1.060 1538.6 1.038 1538.8 1.025 1539.0 1.021 1539.2 1.025 1539.4 1.036 1539.6 1.054 1539.8 1.078 1540.0 1.106 1540.2 1.139 1540.4 1.176 1540.6 1.215 1540.8 1.256 1541.0 1.299 1541.2 1.343 1541.4 1.387 1541.6 1.431 1541.8 1.474 1542.0 1.516 1542.2 1.556 1542.4 1.594 1542.6 1.631 1542.8 1.666 1543.0 1.698 1543.2 1.727 1543.4 1.755 1543.6 1.779 1543.8 1.801 1544.0 1.821 1544.2 1.837 1544.4 1.851 1544.6 1.863 1544.8 1.872 1545.0 1.879 1545.2 1.884 1545.4 1.887 1545.6 1.889 1545.8 1.889 1546.0 1.887 1546.2 1.885 1546.4 1.882 1546.6 1.878 1546.8 1.873 1547.0 1.867 1547.2 1.861 1547.4 1.854 1547.6 1.847 1547.8 1.840 1548.0 1.832 1548.2 1.825 1548.4 1.817 1548.6 1.810 1548.8 1.804 1549.0 1.798 1549.2 1.793 1549.4 1.788 1549.6 1.784 1549.8 1.780 1550.0 1.777 1550.2 1.774 1550.4 1.771 1550.6 1.769 1550.8 1.768 1551.0 1.767 1551.2 1.767 1551.4 1.768 1551.6 1.770 1551.8 1.773 1552.0 1.777 1552.2 1.782 1552.4 1.788 1552.6 1.793 1552.8 1.800 1553.0 1.806 1553.2 1.812 1553.4 1.819 1553.6 1.825 1553.8 1.831 1554.0 1.837 1554.2 1.843 1554.4 1.848 1554.6 1.853 1554.8 1.858 1555.0 1.862 1555.2 1.865 1555.4 1.867 1555.6 1.868 1555.8 1.866 1556.0 1.863 1556.2 1.858 1556.4 1.851 1556.6 1.842 1556.8 1.830 1557.0 1.816 1557.2 1.799 1557.4 1.781 1557.6 1.759 1557.8 1.735 1558.0 1.708 1558.2 1.678 1558.4 1.645 1558.6 1.609 1558.8 1.570 1559.0 1.528 1559.2 1.484 1559.4 1.436 1559.6 1.386 1559.8 1.332 1560.0 1.276 1560.2 1.216 1560.4 1.153 1560.6 1.086 1560.8 1.015 1561.0 0.940 1561.2 0.860 1561.4 0.777 1561.6 0.690 1561.8 0.600 1562.0 0.506 1562.2 0.410 1562.4 0.312 1562.6 0.210 1562.8 0.106 1563.0 0.000